All products
KM-031Available PFAS-free
Antisoiling on Plastic
UV-curable anti-soiling coating for plastic substrates including PET, PC, and PMMA. Provides self-cleaning properties on polymer surfaces where thermal cure is not feasible.
Refractive index rangen = 1.40–1.52
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040
Specifications
Functions
Anti-soiling
Compatible substrates
PETPCPMMA
Processing methods
SPINDIPROLLGRAVURE
Refractive index range
1.40–1.52
1.162.00
| Property | Value |
|---|---|
| Product code | KM-031 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.40–1.52 |
| Cure type | UV |
| PFAS status | Available PFAS-free |
| Functions | Anti-soiling |
| Compatible substrates | PET, PC, PMMA |
| Processing | SPIN, DIP, ROLL, GRAVURE |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.