All products
KM-030Available PFAS-free
Antisoiling on Glass
Thermal-curable anti-soiling coating for glass substrates. Reduces surface contamination and simplifies cleaning in architectural, automotive, and solar panel applications.
Refractive index rangen = 1.40–1.52
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-001–040
Specifications
Functions
Anti-soiling
Compatible substrates
Glass
Processing methods
SPINDIPSPRAY
Refractive index range
1.40–1.52
1.162.00
| Property | Value |
|---|---|
| Product code | KM-030 |
| Chemistry family | Solvent sol-gel |
| Refractive index range | 1.40–1.52 |
| Cure type | Thermal |
| PFAS status | Available PFAS-free |
| Functions | Anti-soiling |
| Compatible substrates | Glass |
| Processing | SPIN, DIP, SPRAY |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related applications
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.