KM-022Available PFAS-free
Anti-Block HC
Hard coating with anti-blocking properties to prevent film-to-film adhesion during roll storage and handling. Essential for R2R production lines processing optical films.
Refractive index rangen = 1.48–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040
Specifications
Functions
Hard coating
Compatible substrates
PETTAC
Processing methods
ROLLGRAVURESLOT DIER2R
Refractive index range
1.48–1.55
1.162.00
| Property | Value |
|---|---|
| Product code | KM-022 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.48–1.55 |
| Cure type | UV |
| PFAS status | Available PFAS-free |
| Functions | Hard coating |
| Compatible substrates | PET, TAC |
| Processing | ROLL, GRAVURE, SLOT DIE, R2R |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related applications
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.