All products
KM-016Available PFAS-free

AS AG 1-Pot

Single-pot UV-curable coating combining antistatic and anti-glare functions. Ideal for display applications where both dust prevention and glare reduction are needed without multi-layer complexity.

Refractive index rangen = 1.48–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040

Specifications

Functions

AntistaticAnti-glare

Compatible substrates

PETPCTAC

Processing methods

SPINDIPROLLGRAVURE

Refractive index range

1.48–1.55
1.162.00
PropertyValue
Product codeKM-016
Chemistry familySolvent UV-curable hybrid
Refractive index range1.48–1.55
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsAntistatic, Anti-glare
Compatible substratesPET, PC, TAC
ProcessingSPIN, DIP, ROLL, GRAVURE
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us