All products
KM-015Available PFAS-free

1-Pot AS AF HC Thermal

Triple-function thermal-curable coating combining hard coating, antifouling, and antistatic properties. Eliminates three separate coating steps in a single formulation cured by heat alone.

Refractive index rangen = 1.45–1.50
1.162.00
Chemistry familyThermal-curable latex
Cure typeThermal
Product blockKM-001–040

Specifications

Functions

Hard coatingAntifoulingAntistatic

Compatible substrates

GlassPCPMMA

Processing methods

SPINDIPSPRAY

Refractive index range

1.45–1.50
1.162.00
PropertyValue
Product codeKM-015
Chemistry familyThermal-curable latex
Refractive index range1.45–1.50
Cure typeThermal
PFAS statusAvailable PFAS-free · fluorinated version available on request
FunctionsHard coating, Antifouling, Antistatic
Compatible substratesGlass, PC, PMMA
ProcessingSPIN, DIP, SPRAY
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us