All products
KM-014Available PFAS-free
1-Pot AF HC Thermal
Thermal-curable hard coating with integrated antifouling functionality. Delivers hardcoat protection and easy-clean properties in a single thermal cure step without UV exposure.
Refractive index rangen = 1.45–1.50
1.162.00
Chemistry familyThermal-curable latex
Cure typeThermal
Product blockKM-001–040
Specifications
Functions
Hard coatingAntifouling
Compatible substrates
GlassPCPMMACR-39
Processing methods
SPINDIPSPRAY
Refractive index range
1.45–1.50
1.162.00
| Property | Value |
|---|---|
| Product code | KM-014 |
| Chemistry family | Thermal-curable latex |
| Refractive index range | 1.45–1.50 |
| Cure type | Thermal |
| PFAS status | Available PFAS-free · fluorinated version available on request |
| Functions | Hard coating, Antifouling |
| Compatible substrates | Glass, PC, PMMA, CR-39 |
| Processing | SPIN, DIP, SPRAY |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related applications
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.