All products
KM-009Available PFAS-free

Antiglare

Anti-glare coating that diffuses specular reflection to reduce glare from ambient light sources. Tuneable haze levels for different display viewing conditions while maintaining image clarity and contrast.

Refractive index rangen = 1.48–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040

Specifications

Functions

Anti-glare

Compatible substrates

PETPCPMMATACGlass

Processing methods

SPINDIPROLLGRAVURE

Refractive index range

1.48–1.55
1.162.00
PropertyValue
Product codeKM-009
Chemistry familySolvent UV-curable hybrid
Refractive index range1.48–1.55
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsAnti-glare
Compatible substratesPET, PC, PMMA, TAC, Glass
ProcessingSPIN, DIP, ROLL, GRAVURE
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us