All products
KM-008Available PFAS-free

1-Pot AR

Single-pot anti-reflective coating that simplifies production by combining base and top layers into one formulation. Provides broadband reflection reduction on plastic substrates with typical reflection below 2% average.

Refractive index rangen = 1.35–1.60
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040

Specifications

Functions

Anti-reflective

Compatible substrates

PETPCPMMATAC

Processing methods

SPINDIPROLLGRAVURESLOT DIE

Refractive index range

1.35–1.60
1.162.00
PropertyValue
Product codeKM-008
Chemistry familySolvent UV-curable hybrid
Refractive index range1.35–1.60
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsAnti-reflective
Compatible substratesPET, PC, PMMA, TAC
ProcessingSPIN, DIP, ROLL, GRAVURE, SLOT DIE
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us