All products
KM-007Available PFAS-free

Antifouling + Antistatic

Combined antifouling and antistatic functionality in a single UV-curable layer. Delivers WCA >100° and surface resistivity in the 10⁹ range. Eliminates the need for separate coating steps, reducing processing cost and time.

Refractive index rangen = 1.45–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040

Specifications

Functions

AntifoulingAntistatic

Compatible substrates

PETPCTAC

Processing methods

SPINDIPROLLGRAVURE

Refractive index range

1.45–1.55
1.162.00
PropertyValue
Product codeKM-007
Chemistry familySolvent UV-curable hybrid
Refractive index range1.45–1.55
Cure typeUV
PFAS statusAvailable PFAS-free · fluorinated version available on request
FunctionsAntifouling, Antistatic
Compatible substratesPET, PC, TAC
ProcessingSPIN, DIP, ROLL, GRAVURE
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.