All products
KM-005Available PFAS-free
Low Refractive Index
Ultra-low refractive index coating reaching RI as low as 1.16 — the lowest available from any PFAS-free supplier globally. Overcoatable for multi-layer AR stacks. Proven to survive furnace tempering at 630°C and deliver 2.5–4.5× light guiding luminance improvement on glass substrates.
Refractive index rangen = 1.16–1.40
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-001–040
Specifications
Functions
Low RIAnti-reflective
Compatible substrates
GlassPETPCTAC
Processing methods
SPINDIPROLLSPRAY
Refractive index range
1.16–1.40
1.162.00
| Property | Value |
|---|---|
| Product code | KM-005 |
| Chemistry family | Solvent sol-gel |
| Refractive index range | 1.16–1.40 |
| Cure type | Thermal |
| PFAS status | Available PFAS-free |
| Functions | Low RI, Anti-reflective |
| Compatible substrates | Glass, PET, PC, TAC |
| Processing | SPIN, DIP, ROLL, SPRAY |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related case studies
Displays0.41%Haze (vs 0.68% incumbent)ULR coating achieves 0.41% haze vs 0.68% incumbent on polariser filmArchitectural Glass4.5×Luminance improvementLRI coating survives 630°C tempering, delivers 2.5–4.5× light guiding gainDisplays<0.15%Residual reflectanceBroadband reflectance below 0.15% achieved on multi-layer AR stack
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.