All products
KM-003Available PFAS-free
Antifouling
Antifouling coating available as a PFAS-free variant, with water contact angle exceeding 100°. Resists fingerprints and smudges while maintaining optical clarity. Functionalised HSiO₂ nanoparticles provide durable easy-clean properties without perfluorinated chemistry.
Refractive index rangen = 1.40–1.50
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040
Specifications
Functions
AntifoulingAnti-smudge
Compatible substrates
PETPCPMMATACGlass
Processing methods
SPINDIPROLLGRAVURE
Refractive index range
1.40–1.50
1.162.00
| Property | Value |
|---|---|
| Product code | KM-003 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.40–1.50 |
| Cure type | UV |
| PFAS status | Available PFAS-free · fluorinated version available on request |
| Functions | Antifouling, Anti-smudge |
| Compatible substrates | PET, PC, PMMA, TAC, Glass |
| Processing | SPIN, DIP, ROLL, GRAVURE |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related case studies
Displays — Foldable200kFold cycles passedSingle-layer hardcoat passes 200,000 fold cycles with PFAS-free anti-smudgeDisplays — ULR0.3×Reflection vs referenceARAF nanoparticle composition achieves 0.3× reference reflection levelDisplays — Foldable>100°Water contact angle (PFAS-free)PFAS-free flexible AR achieves WCA >100° with better retention than PFAS
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.