Eyewear

Safety glasses and visors

Polycarbonate that must stay clear in dust and daily wiping

Safety glasses and visors are polycarbonate, chosen for impact strength — and polycarbonate is soft and charges easily. The standards allow two optional marks on the lens that buyers look for: resistance to surface damage by fine particles, and resistance to fogging. The first is a hard coat. Dust that clings to a charged lens gets wiped across it, so a hard coat that also bleeds off charge protects itself.

OUTSIDEEYE SIDEEasy-clean topcoatOuter faceAntistatic hard coat, outer faceMark K: resistance to surface damage by fineparticlesPolycarbonate lens or visorn 1.59Hard coat, inner faceAnti-fog coating, inner faceMark N: resistance to fogging · not KriyaK2K1K1
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (5)
  1. Easy-clean topcoat Outer faceK2
  2. Antistatic hard coat, outer face Mark K: resistance to surface damage by fine particlesK1
  3. Polycarbonate lens or visor n 1.59
  4. Hard coat, inner faceK1
  5. Anti-fog coating, inner face Mark N: resistance to fogging · not Kriya

Working method

Version 1 · first published

An antistatic hard coat on both faces and an easy-clean layer outside; the anti-fog layer inside is a different chemistry.

Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.

  1. Antistatic hard coat on both faces

    Pencil hardness 3H+ to 4H on polycarbonate; surface resistance 10⁶–10¹² Ω/sq.

    Layers: Antistatic hard coat, outer face · Hard coat, inner face
  2. Easy-clean top layer on the outer face

    Water contact angle above 100° without fluorinated chemistry.

    Layers: Easy-clean topcoat
  3. Anti-fog layer on the inner face

    Not Kriya. The hard coat underneath has to accept it.

    Layers: Anti-fog coating, inner face

Public basis

Earlier public documents that describe the same steps.

Stays with the device maker

Lens or visor moulding, marking and certification.

A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.

Public references

  1. BSI white paper: Protective Eyewear suite of standards — BS EN ISO 16321-1, -2 and -3 — EN ISO 16321 replaces EN 166; optional requirements and lens marking
  2. US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998 patent: UV-curable transparent coating made antistatic with conductive tin-oxide powder, for substrates such as polycarbonate
  3. EP 0 232 033 — Transparent electrically conductive plastic molded articles — 1987 publication: transparent, abrasion-resistant antistatic coat with tin-oxide powder on plastic mouldings
  4. US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993 patent: spin-coated hard coat on plastic ophthalmic lenses, cured by ultraviolet light

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.