A LiDAR fires near-infrared pulses — usually at 905 nm or 1550 nm — through a cover, often an infrared-transparent, visibly black polycarbonate, and catches the echo through the same cover. Each bare PC surface reflects about 5 %, and the light crosses the cover twice: on the way out and on the way back.
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (5)
- AR topcoat — low index n ≈ 1.30 · UV-curable · thickness set for 905 or 1550 nmK1
- AR basecoat — high index n ≈ 1.75 · UV-curable · ≈ 3 µmK1
- Polycarbonate cover IR-transparent, visibly black · n ≈ 1.58
- AR on the inner face Sensor-cavity sideK2
- LiDAR emitter and receiver 905 nm or 1550 nm
Public references
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.