Industrial and hazardous-area light: optic and cover

In an LED luminaire the light passes a secondary optic and an outer cover, usually polycarbonate. Each bare surface reflects about 5 %, scratches and dirt scatter the beam, and in explosive atmospheres a plastic cover that charges up can discharge as a spark. A thin wet coating can carry hard coat, antistatic and anti-reflection on the same part.

LIGHT OUTLED BOARDAntistatic hard coat, outer faceControlled surface resistance + scratchresistance (antistatic AR as an option)Cover or integral lensPolycarbonate · n 1.58 · often part of theenclosureAnti-reflection, inner faceProtected sideAirSecondary opticTIR lens or lens array · PMMA or PCLED packagesPhosphor-converted white LEDs · not KriyaMetal-core board and heat sinkNot KriyaK1K2
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (6)
  1. Antistatic hard coat, outer face Controlled surface resistance + scratch resistance (antistatic AR as an option)K1
  2. Cover or integral lens Polycarbonate · n 1.58 · often part of the enclosure
  3. Anti-reflection, inner face Protected sideK2
  4. Secondary optic TIR lens or lens array · PMMA or PC
  5. LED packages Phosphor-converted white LEDs · not Kriya
  6. Metal-core board and heat sink Not Kriya

Public references

  1. IEC 60079-0:2026 Explosive atmospheres — Part 0: Equipment — General requirements — clause 7.4: electrostatic charges on external non-metallic materials (contents preview)
  2. The non-metallic materials used in equipment for ATEX zones according to the IEC/EN 60079-0 standard — reducing the surface resistivity below 10⁹ Ω is one option against electrostatic charge

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.