Automotive

Automotive cockpit display

Curved cover glass over centre and driver displays

Cockpit displays sit behind large, often curved cover glass that has to stay readable in direct sun, survive daily touch and not mirror the car's interior. Anti-glare, anti-reflection and easy-clean are the usual surface treatments, on one or both faces of the glass.

DRIVERDISPLAY MODULEEasy-clean topcoatFluorine-free optionAnti-reflection coatingGraded high-/low-index layersAnti-glare layerCoated (or etched) diffusing surfaceCurved cover glassAluminosilicate, hot- or cold-formed · n ≈ 1.5Optical bonding resinNot KriyaTouch sensorNot KriyaPolarizerNot KriyaLCD or OLED panelNot KriyaBacklight (local-dimming mini-LED)Not KriyaK3K1K2
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (9)
  1. Easy-clean topcoat Fluorine-free optionK3
  2. Anti-reflection coating Graded high-/low-index layersK1
  3. Anti-glare layer Coated (or etched) diffusing surfaceK2
  4. Curved cover glass Aluminosilicate, hot- or cold-formed · n ≈ 1.5
  5. Optical bonding resin Not Kriya
  6. Touch sensor Not Kriya
  7. Polarizer Not Kriya
  8. LCD or OLED panel Not Kriya
  9. Backlight (local-dimming mini-LED) Not Kriya

Public references

  1. ISO 15008:2017 Road vehicles — Ergonomic aspects of transport information and control systems — Specifications and test procedures for in-vehicle visual presentation — minimum requirements for the image quality and legibility of displays shown to the driver
  2. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.