Energy, buildings & agriculture

CIGS thin-film solar cell

Nanoimprinted moth-eye texture on the front contact

In a CIGS cell, sunlight enters through a transparent AZO front contact (n 1.913 at 633 nm). A sub-wavelength moth-eye texture, imprinted in a resin of almost the same index, grades the step from air into the cell: fewer photons are reflected and more generate current. This is Kriya's peer-reviewed nanoimprint result.

SUNSUBSTRATEMoth-eye textureUV-nanoimprinted Kriya high-index resist ·n 1.792 at 633 nmAZO front contactTransparent conductor · n 1.913 at 633 nmi-ZnO / CdS bufferNot KriyaCIGS absorber0.85–2.0 µm in the studyMolybdenum back contactNot KriyaGlass substrateNot KriyaK1
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (6)
  1. Moth-eye texture UV-nanoimprinted Kriya high-index resist · n 1.792 at 633 nmK1
  2. AZO front contact Transparent conductor · n 1.913 at 633 nm
  3. i-ZnO / CdS buffer Not Kriya
  4. CIGS absorber 0.85–2.0 µm in the study
  5. Molybdenum back contact Not Kriya
  6. Glass substrate Not Kriya

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.