AR & VR

AR headset — curved visor combiner

Displays above the eyes, image reflected by the visor

The simplest see-through display projects the image from displays above the eyes onto a large curved visor. A semi-reflective coating on the inside of the visor sends the image to the eyes; the outside surface sends a second, shifted copy. On a visor this ghost is strong: the mirror is weak, so most of the light reaches the outer surface.

WORLD SIDEEYE SIDEEasy-clean top layerOuter faceHard coat and AR, outer faceConvex side of the visorPolycarbonate visorInjection-moulded · n 1.59Semi-reflective coatingEven thickness over the inner face · about40 % · vacuum dielectric stack, not KriyaAirDisplays and lenses above the eyesNot KriyaK2K1
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (5)
  1. Easy-clean top layer Outer faceK2
  2. Hard coat and AR, outer face Convex side of the visorK1
  3. Polycarbonate visor Injection-moulded · n 1.59
  4. Semi-reflective coating Even thickness over the inner face · about 40 % · vacuum dielectric stack, not Kriya
  5. Displays and lenses above the eyes Not Kriya

Working method

Version 1 · first published

Hard coat, AR and easy-clean on the outer face; one mirror of even thickness on the inner face.

Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.

  1. Hard coat with AR on the outer face

    Hard coat 3H+ to 4H; two-layer UV-curable AR on polycarbonate, high index ≈ 1.75 under low index ≈ 1.30. Behind a 40 % mirror the ghost falls from 4.6 % of the image to 0.9 % at R = 1 % and 0.14 % at R < 0.15 %.

    Layers: Hard coat and AR, outer face
  2. Easy-clean top layer

    Water contact angle above 100° without fluorinated chemistry.

    Layers: Easy-clean top layer
  3. Mirror of even thickness on the inner face

    Vacuum coating over the whole face, about 40 %. Not Kriya.

    Layers: Semi-reflective coating

Public basis

Earlier public documents that describe the same steps.

Stays with the device maker

Mirror design and reflectance, visor shape and display optics.

A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.

Public references

  1. US 3,870,405 — Helmet sight visors — 1975 patent: visor with a partially reflective inner surface; the ghost image comes from the outer surface
  2. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.