Hands-on exercises

Three short tasks in the Tolerance Monte Carlo. Each one gives you the inputs; you report the number.

This tool doesn’t accept URL parameters, so the “Open in tool” buttons below open the tool at its landing page. Set the inputs listed in each exercise by hand.

Yield on the reference quarter-wave

Run the Tolerance Monte Carlo on the 99.6 nm MgF₂ quarter-wave on a 1.52 substrate with production-realistic tolerances, and report the fraction of coatings that meet a standard broadband AR spec.

Inputs to set
  • Layer: 99.6 nm, n = 1.38, tol_d = 10 nm, tol_n = 0.02
  • Substrate: n = 1.52
  • Wavelengths: 450–650 nm
  • Samples: 1000, seed: 42
  • Target: R ≤ 1.5 % across 450–650 nm
Open in tool ↗Open the Tolerance Monte Carlo. Set the single layer to 99.6 nm MgF₂ (<i>n</i> = 1.38) with thickness tolerance 10 nm and index tolerance 0.02. Use substrate <i>n</i> = 1.52, wavelengths 450–650 nm, seed 42, 1 000 samples. Set the target band to R ≤ 1.5 % across 450–650 nm. Report the yield in %.

Tighten the thickness tolerance

Repeat the previous exercise with half the thickness tolerance and show the yield lift.

Inputs to set
  • Layer: 99.6 nm, n = 1.38, tol_d = 5 nm, tol_n = 0.02
  • Substrate: n = 1.52
  • Wavelengths: 450–650 nm
  • Samples: 1000, seed: 42
  • Target: R ≤ 1.5 % across 450–650 nm
Open in tool ↗Same setup as ex-1, but change the thickness tolerance from 10 nm to <strong>5 nm</strong>. Keep index tolerance at 0.02, seed 42, 1 000 samples, target R ≤ 1.5 % across 450–650 nm. Report the new yield.

Read σ(R) at 550 nm

Same run as ex-1, but this time read the per-wavelength standard deviation at the design wavelength. This is the number that sets the ±2σ datasheet envelope.

Inputs to set
  • Layer: 99.6 nm, n = 1.38, tol_d = 10 nm, tol_n = 0.02
  • Substrate: n = 1.52
  • Wavelengths: 450–650 nm, read at 550 nm
  • Samples: 1000, seed: 42
Open in tool ↗Open the Tolerance Monte Carlo with the reference quarter-wave (99.6 nm MgF₂, tol_d = 10 nm, tol_n = 0.02, substrate 1.52, wavelengths 450–650 nm, seed 42, 1 000 samples). Instead of yield, read the standard deviation σ(R) at 550 nm. Report in %.