Three short tasks in the TMM Thin-Film Reflectance Simulator. Each one gives you the inputs; you report the number.
Bare BK7 reflectance at 550 nm
Set up a glass substrate with no coating layers and read off the front-surface reflectance at 550 nm.
Inputs to set
No layers
Substrate: BK7 glass
λ = 550 nm
Angle = 0°
Open in tool ↗Report the reflectance at 550 nm in percent, to two decimal places.
Ideal single-layer AR on BK7
Put an ideal single-layer AR on BK7: n = √(n₀·nₛ), d = λ₀/(4n), target 550 nm. Compute the resulting reflectance at 550 nm.
Inputs to set
Layer 1: n = 1.233, d = 112 nm
Substrate: BK7
λ = 550 nm
Angle = 0°
Open in tool ↗Report R(550 nm) in percent, to three decimal places.
MgF₂ single-layer AR on BK7 — the practical case
MgF₂ (n = 1.38) is the lowest-index solid film that is manufacturable, and it is the industry’s cheapest AR. Put one quarter-wave of MgF₂ on BK7 at 550 nm and report R(550 nm).
Inputs to set
Layer 1: n = 1.380, d = 100 nm (nd ≈ λ/4 at 552 nm)
Substrate: BK7
λ = 550 nm
Open in tool ↗Report R(550 nm) in percent, to two decimal places.