For x ≪ 1 and |mx| ≪ 1 the Mie series is dominated by the a1 dipole term. Expanding:
That is the Rayleigh-Gans limit of Mie theory. The (m²−1)/(m²+2) factor is the Clausius-Mossotti polarisability of a sphere — the same factor that sits inside Maxwell-Garnett.
The (d/λ)⁴ price
Halve the particle diameter and scattering drops 16×. Double the wavelength and scattering drops 16×. That is why visible haze in a filled film is set by the biggest particles (or agglomerates), not the average, and why NIR scatter can be ignored for a visible-band AR design.
When Rayleigh breaks
The expansion fails when x·|m| ≳ 0.5 — larger particles, higher-index particles, shorter wavelengths. The tool's full BHMIE sum covers both regimes; Rayleigh is only used as a sanity check at the small-x end.