Hands-on exercises

Three short tasks in the Angle-Dependent Fresnel Explorer. Each one gives you the inputs; you report the number.

Normal-incidence reflectance of air→BK7

Load the Air → Glass (BK7) preset and read off the single-surface, normal-incidence reflectance.

Inputs to set
  • n₁ = 1.000 (air)
  • n₂ = 1.520 (BK7)
  • k₂ = 0
  • direction = forward
Open in tool ↗Report the unpolarised reflectance at 0° in percent, to two decimal places.

Brewster angle at an air→PMMA interface

Set up an air → PMMA interface. Find the angle at which the p-polarised reflectance is zero.

Inputs to set
  • n₁ = 1.000 (air)
  • n₂ = 1.4915 (PMMA, 589 nm)
  • k₂ = 0
Open in tool ↗Report the Brewster angle in degrees, to one decimal place.

Reflectance of silicon at 60°

Set up an air → silicon interface and compute the unpolarised reflectance at 60°.

Inputs to set
  • n₁ = 1.000 (air)
  • n₂ = 3.480 (silicon, ≈ 550 nm)
  • k₂ = 0.010
Open in tool ↗Report the unpolarised reflectance at 60° in percent, to one decimal place.