AR on the top surface

The Airy single-layer R the tool adds, and what it changes.

Lesson 5 of 5 · ~7 min read

A bare top surface reflects about 3.96 % at normal incidence for PMMA (n = 1.49) and about 4.26 % for glass (n = 1.52). A quarter-wave MgF₂ AR coating takes that to ~1.3 % at 550 nm.

What the AR actually buys

  • Perceived brightness rises by the drop in top-surface loss — about 3 % on PMMA.
  • Ghost suppression is a real second-order effect: the second image comes from back-and-front doubled reflection; AR on the top drops its brightness by the same factor.
  • Chromatic bias: a quarter-wave AR is tuned at one wavelength; off-centre you may get a faint blue or green cast in the reflection. The tool renders the full spectrum so you see it.

Interaction with the extraction pattern

AR on the top surface does not change the uniformity score materially — min and max both scale by the same (1 − Rtop) factor. It changes luminance, not uniformity. For a given spec it often lets you drop the LED current by a few per-cent and recover the equivalent in battery life.