Hands-on exercises

Three short tasks in the Ellipsometry Inversion. Each one gives you the inputs; you report the number.

This tool doesn’t accept URL parameters, so the “Open in tool” buttons below open the tool at its landing page. Set the inputs listed in each exercise by hand.

Cauchy n at 550 nm

Evaluate a two-term Cauchy fit at the design wavelength.

Inputs to set
  • A: 1.46
  • B: 3600 nm²
  • C: 0
  • λ: 550 nm
Open in tool ↗Open Ellipsometry Inversion. Enter Cauchy coefficients A = 1.46, B = 3600 nm², C = 0. Read n(550 nm).

Urbach k at 550 nm

Evaluate the Urbach-like absorption model at the same wavelength.

Inputs to set
  • k₀: 0.001
  • k₁: 400 nm²
  • λ: 550 nm
  • Clamp: non-negative
Open in tool ↗Set k₀ = 0.001 and k₁ = 400 nm². Report k(550 nm).

Forward tan(Ψ) at a known stack

Compute the forward-model tan(Ψ) at 550 nm for a specific thin film on fused silica.

Inputs to set
  • Cauchy A: 1.46
  • Cauchy B: 3600
  • Thickness: 100 nm
  • Substrate: fused silica (n = 1.457)
  • Angle: 70°
Open in tool ↗Set the film to A = 1.46, B = 3600, C = 0, k = 0, d = 100 nm. Substrate fused silica (n = 1.457). Angle 70°. Read tan(Ψ) at 550 nm.