Toutes les études de cas
Écrans — ULR

La composition ARAF de nanoparticules atteint 0,3× le niveau de réflexion de référence

Un fabricant japonais de films AR de premier plan

Indicateurs clés

0.3×Réflexion vs référence
95.6%Transmission totale
0.5%Haze
PassAntisalissure (test marqueur)

01

Le défi

The AR film manufacturer needed a nanoparticle ARAF composition that could achieve ultra-low reflection significantly below their internal reference level, while maintaining acceptable haze and anti-smudge properties for premium display applications.

02

Notre approche

Kriya developed ARAF nanoparticle compositions in two particle sizes (50 nm for low reflection, 75 nm for super-low reflection). Multiple formulation versions were tested at the manufacturer’s facility against their internal reference samples, measuring reflection, haze, transmission, steel wool abrasion, and anti-smudge performance.

03

Le résultat

The 75 nm super-low-reflection variant achieved reflection at 0.3× the reference level with 95.6% total transmission and 0.5% haze. The 50 nm low-reflection variant achieved 0.7× reference reflection with improved abrasion resistance. Both variants passed anti-smudge (fingerprint and marker wipe-off) testing.

Pourquoi Kriya

Kriya’s tuneable nanoparticle platform enables precise control over the reflection–abrasion trade-off, allowing customers to select the optimal balance for their application.

Indicateurs clés

0.3×Réflexion vs référence
95.6%Transmission totale
0.5%Haze
PassAntisalissure (test marqueur)

Produits utilisés

Application associée

Displays — ULR →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.

Démarrer une conversation