Alle Fallstudien
Displays — ULR

ARAF-Nanopartikelkomposition erreicht 0,3× des Referenz-Reflexionsniveaus

Ein führender japanischer AR-Folienhersteller

Kennzahlen

0.3×Reflexion vs. Referenz
95.6%Gesamttransmission
0.5%Trübung
PassAnti-Fingerprint (Marker-Abwischtest)

01

Die Herausforderung

The AR film manufacturer needed a nanoparticle ARAF composition that could achieve ultra-low reflection significantly below their internal reference level, while maintaining acceptable haze and anti-smudge properties for premium display applications.

02

Unser Ansatz

Kriya developed ARAF nanoparticle compositions in two particle sizes (50 nm for low reflection, 75 nm for super-low reflection). Multiple formulation versions were tested at the manufacturer’s facility against their internal reference samples, measuring reflection, haze, transmission, steel wool abrasion, and anti-smudge performance.

03

Das Ergebnis

The 75 nm super-low-reflection variant achieved reflection at 0.3× the reference level with 95.6% total transmission and 0.5% haze. The 50 nm low-reflection variant achieved 0.7× reference reflection with improved abrasion resistance. Both variants passed anti-smudge (fingerprint and marker wipe-off) testing.

Warum Kriya

Kriya’s tuneable nanoparticle platform enables precise control over the reflection–abrasion trade-off, allowing customers to select the optimal balance for their application.

Kennzahlen

0.3×Reflexion vs. Referenz
95.6%Gesamttransmission
0.5%Trübung
PassAnti-Fingerprint (Marker-Abwischtest)

Verwendete Produkte

Verwandte Anwendung

Displays — ULR →

Eine ähnliche Anwendung besprechen

Unser technisches Team hilft Ihnen bei der Bewertung, ob dieser Ansatz für Ihre Anforderungen geeignet ist.

Gespräch beginnen