A foldable phone cannot use rigid cover glass. Its cover is a thin polyimide (CPI) or PET film, often over ultra-thin glass, and that cover must carry hardness, anti-reflection and easy-clean in layers that survive folding many times a day. Wet nanocomposite coatings stay flexible where brittle sputtered stacks crack.

VIEWER SIDEBACK OF THE PANELEasy-clean topcoatFluorine-free, hollow-silica based · n ≈ 1.40Anti-reflection layersHigh-index + low-index stack · n 1.16–1.95Foldable hard coatUV-cured nanocomposite on the cover filmCover filmColourless polyimide (CPI) or PET · coverwindow 30–200 µmOptically clear adhesiveNot KriyaUltra-thin glass (in UTG designs)≈ 30–70 µmOptically clear adhesiveNot KriyaCircular polarizerSuppresses ambient reflection from the metalelectrodesTouch sensorMetal mesh, on-cellThin-film encapsulationInorganic/organic barrierOLED emittersRed, green, blue subpixels · organic layersn ≈ 1.7–1.9TFT backplane on polyimideLTPS / LTPOBack film and support plateNot KriyaK1K2K3
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (13)
  1. Easy-clean topcoat Fluorine-free, hollow-silica based · n ≈ 1.40K1
  2. Anti-reflection layers High-index + low-index stack · n 1.16–1.95K2
  3. Foldable hard coat UV-cured nanocomposite on the cover filmK3
  4. Cover film Colourless polyimide (CPI) or PET · cover window 30–200 µm
  5. Optically clear adhesive Not Kriya
  6. Ultra-thin glass (in UTG designs) ≈ 30–70 µm
  7. Optically clear adhesive Not Kriya
  8. Circular polarizer Suppresses ambient reflection from the metal electrodes
  9. Touch sensor Metal mesh, on-cell
  10. Thin-film encapsulation Inorganic/organic barrier
  11. OLED emitters Red, green, blue subpixels · organic layers n ≈ 1.7–1.9
  12. TFT backplane on polyimide LTPS / LTPO
  13. Back film and support plate Not Kriya