Displays — Faltbar

Einschicht-Hartbeschichtung besteht 200.000 Faltzyklen mit PFAS-freiem Anti-Fingerprint

Ein großer koreanischer Display-Tier-1

Kennzahlen

200kFaltzyklen bestanden
3HPencil hardness
2,000xStahlwolle-Zyklen bestanden
>95°WCA nach Abrieb

01

Die Herausforderung

The OEM required a multi-functional coating for foldable displays that combined hard coating, antistatic, and antifouling properties in a single layer. The coating had to survive 200,000 fold cycles at 1.5R radius without cracking or loss of surface properties, and had to be PFAS-free to meet upcoming regulatory requirements.

02

Unser Ansatz

Kriya formulated a UV-curable multi-functional coating (35 wt% solids) on 75 µm PET, combining hard coating, antistatic (10⁹ Ω/sq), and antifouling (WCA 110°) in a single layer. The coating was validated through exhaustive QC including 2,000-cycle steel wool abrasion, ballpoint pen drop tests, and permanent marker wipe-off testing.

03

Das Ergebnis

The coating passed all qualification criteria: pencil hardness 3H, surface resistivity 8.0×10⁹ Ω/sq, WCA retained above 95° after 2,000 steel wool cycles at 1 kg/cm², and permanent marker wipe-off confirmed. The coating passes 200,000 fold cycles at 1.5R, compatible with R2R processing for volume production.

Warum Kriya

Kriya delivered three functions in one PFAS-free layer, eliminating separate coating steps and reducing both processing cost and regulatory risk for the OEM’s foldable product line.

Kennzahlen

200kFaltzyklen bestanden
3HPencil hardness
2,000xStahlwolle-Zyklen bestanden
>95°WCA nach Abrieb

Verwendete Produkte

Verwandte Anwendung

Displays — Foldable →

Eine ähnliche Anwendung besprechen

Unser technisches Team hilft Ihnen bei der Bewertung, ob dieser Ansatz für Ihre Anforderungen geeignet ist.

Gespräch beginnen