Topfzeit-Timer

How long before this two-pack formulation gels?

Übersetzt die Topfzeit aus dem Datenblatt bei einer Referenztemperatur in das realistische Verarbeitungsfenster bei aktueller Werkstattemperatur via Arrhenius-Kinetik.

How it works

A two-pack resin and hardener start to react as soon as they are mixed; the mixture's viscosity rises until the formulation can no longer be applied. The usable time, or pot life, depends on the mixing ratio, the ambient temperature and the catalyst level. It is shorter in a warm room than in a cool one.

Worked example

Arrhenius E_a 60 kJ/mol — doubling every 10 K

Arrhenius extrapolation of pot life from a reference temperature.

Validation method, references and test-case results: /validation#pot-life

Request accessOpen the interactive tool