Panoramic glass roof

Edge-lit illumination and solar heat control in one laminate

An illuminated roof uses one glass ply as a light guide, fed by LEDs at its edge and lit up by printed or laser-etched extraction patterns. PVB (n 1.48) is almost index-matched to glass (n 1.52), so in a laminate the light leaks into the interlayer within a few bounces. A thin low-index layer restores total internal reflection — and the same PVB can carry ATO to absorb solar heat.

OUTSIDE / SUNCABINOuter glassTinted or privacy glass · n 1.52PVB interlayer with ATOn 1.48 · near-infrared absorberLow-index claddingn ≈ 1.20 · ≈ 1 µmInner glass = light guideLow-iron glass · LEDs at the edgeLight-extraction patternPrinted or laser-etchedLow-E coating (optional)Not KriyaK1K2
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (6)
  1. Outer glass Tinted or privacy glass · n 1.52
  2. PVB interlayer with ATO n 1.48 · near-infrared absorberK1
  3. Low-index cladding n ≈ 1.20 · ≈ 1 µmK2
  4. Inner glass = light guide Low-iron glass · LEDs at the edge
  5. Light-extraction pattern Printed or laser-etched
  6. Low-E coating (optional) Not Kriya

Referenzen

  1. US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
  2. EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder

Schematisch, nicht maßstabsgetreu.