How thick must the wet coat be to leave this dry film thickness?
Voorspelt natte filmdikte uit applicatorinstellingen: Mayer-bar, slot-die, gravure of spincoaten.
How it works
The dry film thickness of a coating equals the wet film thickness multiplied by the volume solids fraction of the formulation. The volume solids fraction follows from the solvent mass fraction, the formulation density and the solvent density. Coating-method process windows set the practical range of wet thickness.
Worked example
Slot-die on 1 m web at 10 m/min, 50 ml/min metered flow → 5 µm wet
Mass-balance wet thickness for Mayer bar, slot-die, gravure or spin.