Kwaliteit & Productie
Van nanodeeltjessynthese via dispersieformulering tot eindcoatingproducten — de gehele waardeketen wordt onder één dak beheerd. ISO 9001:2015 gecertificeerd.
>100k kg/yr
Dispersion capacity
1M kg/yr
Coating capacity designed
0.8 μm
Batch filtration
Tot 10 CTQ
Kwaliteitsparameters per batch
Tot 6 mnd
Houdbaarheid indien niet anders overeengekomen (ongeopend)
Vereenvoudigd productieproces
Verticaal geïntegreerd, volledig beheerst
Elke stap van nanodeeltjessynthese tot eindverpakt product wordt intern beheerst. Kwaliteitsinspectie wordt bij elke stap toegepast conform onze ISO-werkprocedures.
Nanoparticle Synthesis
Synthesis of SiO₂, TiO₂, SnO₂, and ATO nanoparticles. Controlled particle size and narrow distribution.
Dispersion Formulation
Nanoparticles dispersed in solvent or monomer matrices at precise loading levels. Stability engineering and sub-micron filtration to ensure optical clarity.
Quality Testing
Each batch tested against up to 10 CTQ parameters before release. Samples retained for 24 months. Certificate of Analysis issued per batch.
Packaging & Dispatch
Packaging and dispatch. Worldwide shipping available.
Kwaliteitsborging
Tot 10 Kritische Kwaliteitsparameters
Elke productiebatch wordt getest op tot 10 CTQ-parameters vóór vrijgave. Resultaten worden gedocumenteerd in het batch Certificate of Analysis (CoA). De specifieke parameterset is productafhankelijk.
| # | Parameter | Method | Typical Tolerance | Unit |
|---|---|---|---|---|
| 1 | Refractive Index (RI) | Abbe refractometer @ 589 nm | ±0.005 of target | nD |
| 2 | Solids Content | Gravimetric (105°C, 2h) | ±1.0% of target | wt% |
| 3 | Viscosity | Brookfield DV-II+ @ 25°C | ±15% of target | mPa·s |
| 4 | Haze | BYK haze-gard plus | < 0.5% (product dependent) | % |
| 5 | Transmittance | UV-Vis spectrophotometer | > 92% @ 550 nm | %T |
| 6 | Pencil Hardness | ASTM D3363 | ≥ target grade | H scale |
| 7 | Adhesion | Cross-cut tape test (ASTM D3359) | 5B / 4B minimum | Rating |
| 8 | Surface Resistivity | Four-point probe / Hiresta | Within spec range | Ω/sq |
| 9 | Water Contact Angle | Sessile drop goniometer | Per product spec | ° |
| 10 | Shelf Life Stability | Accelerated aging (50°C, 4 weeks) | All params within spec | Pass/Fail |
Productiecapaciteit
Opschaalvermogen
Kriya hanteert een continu opschaalpad van R&D-bank via pilot naar productie, met gedocumenteerde opschaalfactoren per chemiefamilie.
Certificeringen
Certificeringen & standaarden
Kwaliteitsdocumentatie nodig voor uw kwalificatie?
CoA, SDS, REACH-verklaringen en applicatiespecifieke testdata beschikbaar op aanvraag.