Baanspanning-calculator

What web tension suits this coated substrate?

Bepaal veilige baanspanning voor dunne polymeerfilms en aluminiumfolie uit substraattreksterkte, dwarsdoorsnede en een gekozen veiligheidsfactor.

How it works

A coated web must be transported at a tension high enough to avoid wrinkling and low enough to avoid substrate stretch or coating damage. The window is set by the substrate's modulus, the coating's elastic limit and the line geometry. A simple force balance gives the recommended tension for each process station.

Worked example

PET 50 µm × 1 m wide at 60 m/min

Minimum and target web tension from substrate yield and curvature radius.

Validation method, references and test-case results: /validation#web-tension

Request accessOpen the interactive tool