Pot-life Timer
How long before this two-pack formulation gels?
Vertaalt de pot-life op het datasheet bij een referentietemperatuur naar het realistische werkvenster bij de huidige werkplaatstemperatuur via Arrhenius-kinetiek.
How it works
A two-pack resin and hardener start to react as soon as they are mixed; the mixture's viscosity rises until the formulation can no longer be applied. The usable time, or pot life, depends on the mixing ratio, the ambient temperature and the catalyst level. It is shorter in a warm room than in a cool one.
Worked example
Arrhenius E_a 60 kJ/mol — doubling every 10 K
Arrhenius extrapolation of pot life from a reference temperature.
Validation method, references and test-case results: /validation#pot-life