Energie, gebouwen & landbouw

Crystalline-silicon PV module

Front glass that lets more light in and stays clean

About 4 % of the sunlight hitting a module bounces off its front glass before it reaches the cells. A porous low-index layer cuts that reflection; an anti-soiling top coat helps keep dust from eating the gain back.

SUNBACKAnti-soiling top coatOuter faceLow-index anti-reflection layerPorous, PFAS-freeSolar glass3.2 mm · n 1.52EncapsulantEVA or POE · n ≈ 1.48Silicon cells and ribbonsNot KriyaEncapsulantNot KriyaBacksheet or rear glassNot KriyaK1K2
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (7)
  1. Anti-soiling top coat Outer faceK1
  2. Low-index anti-reflection layer Porous, PFAS-freeK2
  3. Solar glass 3.2 mm · n 1.52
  4. Encapsulant EVA or POE · n ≈ 1.48
  5. Silicon cells and ribbons Not Kriya
  6. Encapsulant Not Kriya
  7. Backsheet or rear glass Not Kriya

Schematisch, niet op schaal.