Alle casestudies
Solar & Energy

3.9% transmission gain on photovoltaic cover glass with thermal-curable LRI

A leading solar module integrator

Kerncijfers

+3.9%Transmission gain
93.8%Coated transmission
630°CTempering survived
0.34%Haze

01

De uitdaging

The solar integrator needed an anti-reflective coating for photovoltaic cover glass that could increase module efficiency through higher light transmission. The coating had to survive outdoor weathering (IEC 61215) and be compatible with tempered glass processing.

02

Onze aanpak

Kriya applied thermal-curable LRI coating (RI 1.37) directly to the glass substrate. The coating was tested for transmission gain, haze, and tempering survival. Accelerated weathering was validated per IEC 61215 standards.

03

Het resultaat

The LRI coating delivered 3.9% transmission gain (from 89.9% to 93.8% C-illuminant) with 0.34% haze. The coating survived tempering at 630°C and passed accelerated weathering validation. Direct glass coating eliminates the need for laminated AR films.

Waarom Kriya

Kriya’s thermal-curable LRI uniquely survives glass tempering, enabling direct application in the solar module production line without additional lamination steps.

Kerncijfers

+3.9%Transmission gain
93.8%Coated transmission
630°CTempering survived
0.34%Haze

Gebruikte producten

Gerelateerde toepassing

Solar & Energy →

Bespreek een vergelijkbare toepassing

Ons technisch team helpt u beoordelen of deze aanpak van toepassing is op uw specifieke vereisten.

Start een gesprek