TIR & Escape-Cone-Rechner
How much light escapes the exit interface of a high-index medium?
Grenzwinkel, Austrittsanteil, geführter Anteil und die minimale Hüllschichtdicke — für die tatsächlich vorliegende Geometrie, nicht die Lehrbuchversion.
How it works
Light inside a high-index medium escapes into a lower-index external medium only within the escape cone set by the critical angle of total internal reflection. Isotropic emission inside the high-index medium puts a fixed fraction of its total power into that cone. The escaping fraction depends only on the two refractive indices.
Worked example
Critical angle, glass n 1.52 → air
Inputs: n1 = 1.52, n2 = 1
Result: 41.14 °
Reference: Born & Wolf §1.5.4
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#tir-escape-cone-calculator