Stoney-Spannung & Substratverbiegung
What curvature does a stressed film induce in its substrate?
Berechnen Sie die equibiaxiale Filmspannung aus einer gemessenen Substratkrümmung oder sagen Sie die Waferbiegung für eine Zielspannung voraus. 12 Substratmaterialien.
How it works
Stoney's equation relates the biaxial stress in a thin film to the curvature it induces in a much thicker substrate, given the substrate's biaxial modulus and thickness and the film thickness. The equation assumes an elastic substrate, a uniform film stress and a film-to-substrate thickness ratio below a few percent. Measured curvature therefore gives a direct read-out of residual stress for thin coatings.
Worked example
Si(100), E 130 GPa, ν 0.28, 525 µm substrate, 1 µm film, R 10 m
Inputs: substrate = silicon_100, substrateThicknessUm = 525, filmThicknessNm = 1.000e+3, radiusOfCurvatureM = 10
Result: 829.4 MPa
Reference: Stoney 1909 Proc. R. Soc. A 82, 172; Freund & Suresh 2003 §2.3
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#stoney-stress