Phase, Gruppenlaufzeit & GDD

How much group delay dispersion does this stack add?

Spektrale Phase, Gruppenlaufzeit und Gruppenlaufzeit-Dispersion von Mehrschicht-Beschichtungen. Für Ultrakurzpuls-Spiegel und Breitband-Antireflexbeschichtungen auf Lasersystemen.

How it works

A multilayer stack adds a wavelength-dependent reflection phase on top of its amplitude response. The second derivative of that phase with respect to angular frequency is the group delay dispersion, which stretches a short pulse in time. The transfer-matrix method gives the phase directly from the stack definition.

Worked example

4-layer TiO₂ / SiO₂ chirped-mirror reference stack

GDD computed via d(GD)/dω with Macleod sign convention; parity with the TS↔Python reference under tests/.

Validation method, references and test-case results: /validation#phase-gdd