Metalinsen-Phasenprofil-Designer
How do I design a flat lens from nanopillars?
Entwurf einer polarisationsunabhängigen, transmissiven Metalinse: radiale Phasenkarte erzeugen, Nanopillar-Abstand vorschlagen und MTF in der Brennebene vorhersagen.
How it works
A metalens imposes a position-dependent phase on an incident wavefront using an array of sub-wavelength scatterers. For an ideal thin lens the required phase profile is hyperbolic in the radial coordinate; each scatterer's local geometry selects the phase it imprints. The focal-plane modulation transfer function follows from the achieved phase profile and the scatterer transmission.
Worked example
f 3 mm, Ø 3 mm, λ 532 nm, Kriya HRI pillars
Hyperbolic phase sampled at Nyquist; Airy disk and MTF cutoff from NA.
Validation method, references and test-case results: /validation#metalens