LIDAR-Fenster-Transmissionsrechner
How much signal does the cover window lose for a 905 nm or 1550 nm LiDAR?
Berechnet die Hin- und Rücktransmissions-Verbesserung durch eine Kriya-AR-Beschichtung auf einem LIDAR-Abdeckfenster bei 905, 940 oder 1550 nm.
How it works
A LiDAR cover window sees the emission pulse twice — once outbound, once on the return. Each pass is attenuated by the coated window's transmittance at the laser wavelength, so the signal returned to the detector scales as the square of the single-pass transmittance. A narrow-band anti-reflection coating recovers most of the loss at the design wavelength.
Worked example
Lossless incoherent slab, n 1.52: R_total = 2R / (1 + R)
Inputs: nSlab = 1.52
Result: 8.168 %
Reference: Born & Wolf §1.6.3 — thick-slab incoherent sum
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#lidar-window