How do I invert an ellipsometry spectrum to get n, k and thickness?

Fit von n(λ), k(λ) und d aus spektroskopischen Ellipsometriedaten Ψ, Δ. Single- oder Multi-Angle. Cauchy + Urbach-Dispersionsmodell.

How it works

Spectroscopic ellipsometry measures the amplitude ratio (Ψ) and phase difference (Δ) between s- and p-polarised reflections from a sample. Fitting these two quantities over wavelength to a parametric optical model yields the refractive index, extinction coefficient and layer thickness. Over-parameterised models are regularised by constraining the dispersion to a physically motivated form.

Worked example

Synthetic Cauchy film on BK7

Multi-angle Ψ/Δ inversion with a 3-term Cauchy film + Urbach k on a BK7 substrate.

Validation method, references and test-case results: /validation#ellipsometry