Effective-Medium-Rechner

What refractive index does a nanoparticle-in-matrix mixture have?

Effektiver Brechungsindex von Komposit-, porösen und Nanopartikel-Beschichtungen: vorwärts oder invers, in Vol.-% oder Gew.-%, mit zitiertem Materialkatalog.

How it works

Effective-medium theories model a composite of small inclusions in a host matrix as a homogeneous medium with an averaged dielectric function. Maxwell-Garnett is valid at low filler fractions with isolated inclusions; Bruggeman handles higher loadings where inclusions percolate. The predicted effective index depends on the inclusion volume fraction, the host and inclusion dielectric functions, and the characteristic inclusion size relative to the wavelength.

Worked example

Maxwell–Garnett: air in SiO₂ (n 1.46), f 0.30

Inputs: nHost = 1.46, nInclusion = 1, volumeFraction = 0.3

Result: 1.321

Reference: Maxwell Garnett 1904; Aspnes 1982 Thin Solid Films 89, 249

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#effective-medium

Request accessOpen the interactive tool