Trocknungsprofil-Planer
What drying profile matches this solvent system?
Prüft, ob Ofenlänge, Liniengeschwindigkeit und Temperatur dem Nassfilm genug Verweilzeit zum Trocknen geben, und meldet Untertrocknung, wenn die Verweilzeit unter die Diffusionsschätzung fällt.
How it works
A coating dries as its solvent evaporates by diffusion through a growing dry skin. The drying rate is set by the solvent's volatility, the oven-air relative humidity and the mass-transfer coefficient at the coating surface. Too-fast drying leaves surface defects; too-slow drying leaves residual solvent in the film.
Worked example
Vrentas–Duda free-volume diffusion profile
Zone-by-zone drying time from solvent BP, dwell per zone and line speed.
Validation method, references and test-case results: /validation#drying-profile