Breitband-AR-Stack-Optimierer
Which layer thicknesses minimise reflectance across a target band?
Findet für ein vorgegebenes Wellenlängenband die Schichtdicken, die die mittlere Reflexion minimieren — basierend auf der Kriya-Materialbibliothek.
How it works
Multilayer anti-reflection design minimises the band-averaged reflectance of a stack by varying the thickness of each layer. A forward optical model such as the transfer-matrix method evaluates the reflectance for any trial thickness vector; a global optimiser such as differential evolution searches that space for a minimum subject to layer-count and index constraints.
Worked example
Target R < 0.5 % 420–680 nm on PMMA
4-layer stack from the Kriya LRI 1.35 / HRI 1.65 library.
Validation method, references and test-case results: /validation#ar-optimizer