Alle Fallstudien
Solar & Energie

3,9% Transmissionsgewinn auf PV-Deckglas mit thermisch härtbarem LRI

Ein führender Solarmodul-Integrator

Kennzahlen

+3.9%Transmissionsgewinn
93.8%Beschichtete Transmission
630°CHärtung überstanden
0.34%Trübung

01

Die Herausforderung

The solar integrator needed an anti-reflective coating for photovoltaic cover glass that could increase module efficiency through higher light transmission. The coating had to survive outdoor weathering (IEC 61215) and be compatible with tempered glass processing.

02

Unser Ansatz

Kriya applied thermal-curable LRI coating (RI 1.37) directly to the glass substrate. The coating was tested for transmission gain, haze, and tempering survival. Accelerated weathering was validated per IEC 61215 standards.

03

Das Ergebnis

The LRI coating delivered 3.9% transmission gain (from 89.9% to 93.8% C-illuminant) with 0.34% haze. The coating survived tempering at 630°C and passed accelerated weathering validation. Direct glass coating eliminates the need for laminated AR films.

Warum Kriya

Kriya’s thermal-curable LRI uniquely survives glass tempering, enabling direct application in the solar module production line without additional lamination steps.

Kennzahlen

+3.9%Transmissionsgewinn
93.8%Beschichtete Transmission
630°CHärtung überstanden
0.34%Trübung

Verwendete Produkte

Verwandte Anwendung

Solar & Energy →

Eine ähnliche Anwendung besprechen

Unser technisches Team hilft Ihnen bei der Bewertung, ob dieser Ansatz für Ihre Anforderungen geeignet ist.

Gespräch beginnen