Alle Fallstudien
Displays — Faltbar

PFAS-freie flexible AR erreicht WCA >100° mit besserer Haltbarkeit als PFAS

Ein großer koreanischer Display-Tier-1

Kennzahlen

>100°Wasserkontaktwinkel (PFAS-frei)
SuperiorWCA-Beibehaltung vs. PFAS
PassAnti-Fingerprint-Haltbarkeit
R2RProduktionskompatibel

01

Die Herausforderung

With PFAS regulation tightening globally, the display OEM needed a PFAS-free anti-reflective and anti-fouling solution for foldable displays that could match or exceed the surface property retention of incumbent PFAS-based coatings under repeated mechanical stress.

02

Unser Ansatz

Kriya’s PFAS-free ARAF technology, based on functionalised HSiO₂ nanoparticles, was tested against PFAS-based references for water contact angle, anti-smudge durability, and retention after steel wool abrasion cycles. The formulation was designed for UV cure compatibility with R2R processing.

03

Das Ergebnis

The PFAS-free coating achieved WCA above 100° with superior retention versus PFAS-based alternatives after repeated abrasion. Anti-smudge properties (fingerprint resistance and marker wipe-off) were maintained across the full test protocol. The coating is R2R-compatible for volume production.

Warum Kriya

Kriya provides a complete PFAS-free alternative that actually outperforms PFAS on durability retention, eliminating regulatory risk while improving product performance.

Kennzahlen

>100°Wasserkontaktwinkel (PFAS-frei)
SuperiorWCA-Beibehaltung vs. PFAS
PassAnti-Fingerprint-Haltbarkeit
R2RProduktionskompatibel

Verwendete Produkte

Verwandte Anwendung

Displays — Foldable →

Eine ähnliche Anwendung besprechen

Unser technisches Team hilft Ihnen bei der Bewertung, ob dieser Ansatz für Ihre Anforderungen geeignet ist.

Gespräch beginnen