Breitband-Restreflexion unter 0,15% auf Mehrschicht-AR-Stack erreicht

Ein führender Tier-1-Display-Optikfolienhersteller

Kennzahlen

<0.15%Restreflexion
+3.3%Transmissionsgewinn (PET)
100%Haftung auf allen Substraten
4Validierte Substrate

01

Die Herausforderung

The consumer-electronics company required a broadband anti-reflective coating stack achieving residual reflectance below 0.15% across the visible spectrum. The solution had to be PFAS-free and compatible with their existing substrate portfolio (PET, PC, PMMA, TAC).

02

Unser Ansatz

Kriya designed a multi-layer AR stack utilising the full RI platform from 1.16 to 1.95. The stack was optimised through optical modelling and validated on four substrates, measuring transmission gain, haze, reflection, pencil hardness, and adhesion per ISO and ASTM standards.

03

Das Ergebnis

Broadband residual reflectance below 0.15% was achieved on the multi-layer stack. Transmission gains ranged from 2.2% (PMMA) to 3.3% (PET), with 100% adhesion on all substrates. Pencil hardness varied by substrate from HB (PC) to 4H (PMMA). All formulations were PFAS-free.

Warum Kriya

Kriya offers the widest PFAS-free RI range (1.16–2.00) from a single supplier, enabling complete multi-layer AR stacks without sourcing from multiple vendors.

Kennzahlen

<0.15%Restreflexion
+3.3%Transmissionsgewinn (PET)
100%Haftung auf allen Substraten
4Validierte Substrate

Verwendete Produkte

Verwandte Anwendung

Displays →

Eine ähnliche Anwendung besprechen

Unser technisches Team hilft Ihnen bei der Bewertung, ob dieser Ansatz für Ihre Anforderungen geeignet ist.

Gespräch beginnen