Automobil-Thermik

ATO-Dispersion erreicht 0,2–0,3% Trübung in PVB, validiert durch Tier-1-Zwischenschichtpartner

Ein Tier-1-PVB-Zwischenschichthersteller

Kennzahlen

<0.3%Trübung (Automotive-Qualität)
5×Effektiver vs. Wettbewerber bei gleichem SHGC
~60%Kosten vs. ITO
75%Sichtbare Lichttransmission

01

Die Herausforderung

The Tier-1 PVB interlayer partner needed an ATO dispersion for solar heat control interlayer film that could achieve automotive-grade haze (<0.5%) when laminated with green glass. Previous ATO suppliers using top-down ball-milling produced dispersions with haze exceeding 1.7%, far above automotive requirements.

02

Unser Ansatz

Kriya provided four ATO dispersion variants at 8.3 wt% concentration for evaluation. The partner laminated samples with 2.0 mm green glass and measured optical properties including visible light transmission, total solar transmittance, and haze according to their internal automotive qualification protocol.

03

Das Ergebnis

The optimised variant achieved 0.2% haze at 0.10 wt% and 0.3% haze at 0.20 wt% in PVB—the only samples passing the partner’s automotive haze threshold. Visible light transmission ranged from 71–75%, and total solar transmittance from 58–61%. The partner concluded the technology had "great potential."

Warum Kriya

Kriya’s proprietary bottom-up ATO synthesis produces nanoparticles with fundamentally lower scattering than ball-milled alternatives, achieving 5× better effectiveness at equal SHGC versus the leading competitor.

Kennzahlen

<0.3%Trübung (Automotive-Qualität)
5×Effektiver vs. Wettbewerber bei gleichem SHGC
~60%Kosten vs. ITO
75%Sichtbare Lichttransmission

Verwendete Produkte

Verwandte Anwendung

Automotive Thermal →

Eine ähnliche Anwendung besprechen

Unser technisches Team hilft Ihnen bei der Bewertung, ob dieser Ansatz für Ihre Anforderungen geeignet ist.

Gespräch beginnen