AR & VR

VR / MR headset — pancake optics

Folded light path between display and eye

Pancake optics fold the light path between a 50/50 mirror and a reflective polarizer, so the lens can sit close to the display and the headset gets shorter. The price is stray light: every extra reflection at a lens or film surface can reach the eye as a ghost image. Anti-reflection on every air-facing surface is part of the optical design.

EYE SIDEDISPLAYAR, hard coat and easy-cleanEye-side lens surfaceLens 2Polymer or glassReflective polarizerLaminated filmQuarter-wave plateLaminated filmAR on the film surfaceFacing the folded cavityAir gap (folded cavity)AR on lens 1Cavity sideLens 1 with 50/50 mirrorPartial mirror on the display-side surfaceAR on the display filmFacing lens 1Circular polarizer on the displayPolarizer + quarter-wave filmDisplayMicro-OLED or LCDK1K2K2K3
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (10)
  1. AR, hard coat and easy-clean Eye-side lens surfaceK1
  2. Lens 2 Polymer or glass
  3. Reflective polarizer Laminated film
  4. Quarter-wave plate Laminated film
  5. AR on the film surface Facing the folded cavityK2
  6. AR on lens 1 Cavity sideK2
  7. Lens 1 with 50/50 mirror Partial mirror on the display-side surface
  8. AR on the display film Facing lens 1K3
  9. Circular polarizer on the display Polarizer + quarter-wave film
  10. Display Micro-OLED or LCD

Arbeitsweise

Version 1 · erstmals veröffentlicht

Anti-reflection on every film and lens surface that faces air, from the display to the eye.

Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.

  1. AR on the film and lens surfaces inside the cavity

    Multi-layer AR, R < 0.15 %, applied roll-to-roll on the films.

    Schichten: AR on the film surface · AR on lens 1
  2. AR on the display film

    Light sent back to the display returns as a ghost of 0.25 × the reflectance it meets there: about 1 % of the image for a bare film surface, 0.04 % with R < 0.15 %.

    Schichten: AR on the display film
  3. AR, hard coat and easy-clean on the eye-side lens

    Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.

    Schichten: AR, hard coat and easy-clean

Öffentliche Grundlage

Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.

Bleibt beim Gerätehersteller

Polarizer and wave-plate films, the partial mirror and the lens design.

Diese Beschreibung ist kein juristischer Hinweis.

Referenzen

  1. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
  2. H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition

Schematisch, nicht maßstabsgetreu.