Brillen

Sunglasses — polarized lens

A dark lens makes its own back surface the problem

A sunglass lens is dark by design: a category 3 lens passes 8 to 18 % of the light. That is exactly why its back surface matters. Light arriving from behind or from the side is not dimmed by the lens at all — the bare back surface mirrors about 5 % of it straight into the eye, which can rival the dimmed scene in front. An AR coating on the back surface removes that glare; the front needs a hard coat and an easy-clean layer.

FRONT (WORLD SIDE)BACK (EYE SIDE)Easy-clean topcoatFrontMirror or flash coating (optional)Vacuum · not KriyaHard coat, frontIndex-matched to polycarbonatePolycarbonate sheetProtects the polarizing filmPolarizing filmDyed, stretched PVA · heat-sensitive · notKriyaPolycarbonate sheet and lens bodyTinted · n 1.59Hard coat, backBack-side anti-reflectionFaces the eyeK3K1K1K2
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (8)
  1. Easy-clean topcoat FrontK3
  2. Mirror or flash coating (optional) Vacuum · not Kriya
  3. Hard coat, front Index-matched to polycarbonateK1
  4. Polycarbonate sheet Protects the polarizing film
  5. Polarizing film Dyed, stretched PVA · heat-sensitive · not Kriya
  6. Polycarbonate sheet and lens body Tinted · n 1.59
  7. Hard coat, backK1
  8. Back-side anti-reflection Faces the eyeK2

Arbeitsweise

Version 1 · erstmals veröffentlicht

A UV-cured hard coat matched to polycarbonate, a wet AR on the back surface, an easy-clean layer on the front; no bake after moulding.

Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.

  1. UV-cured hard coat matched to polycarbonate

    Index up to 1.65 (polycarbonate: 1.59). Cured by UV light, so the polarizing film sees no further heat.

    Schichten: Hard coat, front · Hard coat, back
  2. Wet AR on the back surface

    Behind a 12 % lens a bare polycarbonate back surface adds glare worth 43 % of the scene; with R < 0.15 %, about 1 %.

    Schichten: Back-side anti-reflection
  3. Easy-clean top layer on the front

    Water contact angle above 100° without fluorinated chemistry.

    Schichten: Easy-clean topcoat

Öffentliche Grundlage

Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.

Bleibt beim Gerätehersteller

Polarizing film, tint, mirror coating and lens moulding.

Diese Beschreibung ist kein juristischer Hinweis.

Referenzen

  1. ISO 12312-1:2022 Eye and face protection — Sunglasses and related eyewear — Part 1: Sunglasses for general use — filter categories by luminous transmittance; category 3 is 8–18 %
  2. US 5,165,992 — Hard coating film and optical elements having such coating film — 1991 filing: high-index oxide particles in the hard coat suppress interference fringes on high-index plastic lenses
  3. US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993 patent: spin-coated hard coat on plastic ophthalmic lenses, cured by ultraviolet light
  4. US 4,070,097 — Ophthalmic antireflection coatings with metal, dielectric, substrate, metal, dielectric in sequence — 1976 filing: in spectacles the unwanted reflection comes from the back of the lens, so the eye-side coating is built for low reflection seen from the eye

Schematisch, nicht maßstabsgetreu.